Nederlands | Français | English
 
 
 
 
 

Installation


The flexible tube is inserted into the existing chimney, then first with air and afterwards with steam at opprox. 100°C, till the complete plymerization of the thermosetting resin (approx 75-85 min)
 
                 
FASE 1
Videoinspection
  FASE 2
The liner inset and the bush positioning
  FASE 3
Inflation with the forced air
  FASE 4
Polymerization
  FASE 5
Cutting and the work is done